Dual-stabilised · 18% Cr ferritic

439 Stainless Steel

The balanced grade. 18% chromium with titanium and niobium dual stabilisation gives mufflers and converter housings the oxidation resistance they need — without the nickel price of an austenitic alloy.

17.0–19.0%Chromium
Ti + NbDual stabilised
≈ 900 °CMax service
2B · BAFinish

439

Mid-section default

UNS S43035 · EN 1.4510 · JIS SUS 439 · ASTM A240

439 is an 18% chromium ferritic stainless steel stabilised with both titanium and niobium. The dual addition pins carbon and nitrogen as stable precipitates, so the weld zone keeps its corrosion resistance and ductility even in thin gauge.

Compared with 409L it buys roughly 100 °C more oxidation headroom, a noticeably better surface after long service, and improved resistance to the acidic condensate that collects in mufflers. That is why it has become the default material for muffler shells, converter housings and the mid-section pipe on passenger cars and light commercial vehicles.

Why specify 439

  • Oxidation resistance to approximately 900 °C — enough for close-mounted converter shells.
  • Ti + Nb dual stabilisation gives consistent as-welded toughness across the heat-affected zone.
  • Lower thermal expansion than 304, reducing distortion on long welded assemblies.
  • Good resistance to exhaust condensate and chloride-containing road spray.
  • Available in bright annealed (BA) finish for visible end caps and trim.

Chemical composition

Typical ladle analysis, weight % — ASTM A240 / EN 10088-2
ElementCSiMnPSCrNiTiNbN
Range ≤ 0.030≤ 1.00≤ 1.00≤ 0.040≤ 0.030 17.00–19.00≤ 0.500.10–0.350.10–0.60≤ 0.030

Mechanical properties

Typical room-temperature properties, annealed and skin-passed
PropertyYield strength Rp0.2Tensile strength RmElongation A50Hardness
Value≥ 240 MPa≥ 430 MPa≥ 22%≤ 88 HRB

Supply range

FormThicknessWidth / sizeFinish
Cold-rolled coil0.30–3.00 mm600–1,350 mm2B, 2D, BA
Cut sheet0.30–3.00 mm200–6,000 mm length2B, BA
Slit strip0.30–2.00 mm8–1,250 mm2B, BA, edge-conditioned
Welded tube0.40–2.00 mm wall25–120 mm ODAnnealed seam

Processing notes

Welding: use a matching stabilised ferritic filler (ER439 or equivalent). Shielding gas coverage matters more than heat input on thin gauge. Forming: 439 draws and stretches well in the annealed condition; for deep shells we recommend a 2B finish and a drawing lubricant matched to the die. Service: avoid sustained exposure above 900 °C, where grain growth begins to embrittle the ferrite.

For converter housings we routinely supply 439 with a controlled grain size and a documented surface roughness so the matted substrate holds consistently on the wrapping line.

Other grades

Match the alloy
to the position.

409L

UNS S40910
EN 1.4512

Ti-stabilised 11% Cr workhorse for manifolds, downpipes and hot-end tubing.

11% Cr≤ 800 °C
Grade data

436L

UNS S43600
EN 1.4526

1% molybdenum for chloride pitting resistance in road-salt and coastal climates.

1% MoSalt resistant
Grade data

444

UNS S44400
EN 1.4521

18% Cr + 2% Mo, PREN ≈ 24, for EGR coolers and heat exchangers.

2% MoPREN ≈ 24
All grades