Austenitic · 300 series

300 Series Stainless Steel

304, 304L, 316L and 321 in coil, sheet and plate. The general-purpose austenitic range — formable, weldable and available from stock in the finishes your line already runs.

18–20%Chromium
8–12%Nickel
0.30–6.00mm gauge
2B · BA · No.4Finish

304 / 304L

General purpose

UNS S30400 / S30403 · EN 1.4301 / 1.4307 · JIS SUS 304 · ASTM A240

304 is the austenitic stainless steel most fabrication shops standardise on. The 18% chromium, 8% nickel balance gives it enough corrosion resistance for indoor and urban service, and a forming and welding behaviour that needs no special procedure. It deep-draws, bends, polishes and welds predictably — which is why it ends up in sinks, appliance panels, food equipment and architectural trim.

304L is the low-carbon variant. The lower carbon ceiling reduces carbide precipitation in the weld heat-affected zone, so heavy-section welded assemblies do not need a post-weld anneal to keep their corrosion resistance. For sheet under about 3 mm the difference is small; for tube, flanges and repeated welds it matters.

Why specify 300 series

  • Predictable forming: 304 takes deep draws and tight bend radii in the annealed condition.
  • Welds with standard 308L filler — no preheat, no post-weld heat treatment for thin gauge.
  • 2B, BA and No.4 finishes available from stock for visible and non-visible parts.
  • 316L adds 2–3% molybdenum where chlorides, coastal air or cleaning chemicals attack the surface.
  • 321 is titanium-stabilised for welded parts that see elevated temperature in service.

Chemical composition

Typical ladle analysis, weight % — ASTM A240 / EN 10088-2
ElementCSiMnPSCrNiN
304 ≤ 0.07≤ 0.75≤ 2.00≤ 0.045≤ 0.030 18.00–20.008.00–10.50≤ 0.10
304L ≤ 0.030≤ 0.75≤ 2.00≤ 0.045≤ 0.030 18.00–20.008.00–12.00≤ 0.10

Mechanical properties

Typical room-temperature properties, annealed and skin-passed
PropertyYield strength Rp0.2Tensile strength RmElongation A50Hardness
304 / 304L≥ 205 MPa≥ 520 MPa≥ 40%≤ 92 HRB

The rest of the range

GradeCrNiMoWhere it earns its price
304L18.0–20.0%8.0–12.0%—Welded assemblies where carbon pickup is a risk
316L16.0–18.0%10.0–14.0%2.0–3.0%Coastal, chemical and marine service; food plant with chloride cleaning
32117.0–19.0%9.0–12.0%—Ti-stabilised; welded parts at elevated temperature

Supply range

FormThicknessWidth / sizeFinish
Cold-rolled coil0.30–6.00 mm600–1,500 mm2B, BA, No.4
Cut sheet0.30–6.00 mm200–6,000 mm length2B, BA, No.4, hairline
Slit strip0.30–3.00 mm8–1,250 mm2B, edge-conditioned
Welded tube0.40–2.00 mm wall25–120 mm ODAnnealed seam, polished on request

Processing notes

Welding: 308L filler for 304 and 304L, 316L filler for 316L. No preheat; keep interpass temperature below 150 °C on thin sheet to limit distortion. Forming: annealed 304 draws well, but it work-hardens — plan an intermediate anneal for multi-stage draws. Finishing: weld discolour must be removed and passivated if the part is visible or exposed to chlorides.

Coil and sheet ship with the mill's EN 10204 3.1 certificate, a dimensional report and — on request — PMI verification per heat. PVC film, interleaving paper and fumigated export packing are arranged before loading.

Other products

Match the alloy
to the job.

409L

UNS S40910
EN 1.4512

Ti-stabilised 11% Cr workhorse for manifolds, downpipes and hot-end tubing.

11% Cr≤ 800 °C
Grade data

439

UNS S43035
EN 1.4510

18% Cr, Ti + Nb stabilised. Mufflers, converter shells and mid-section pipe.

18% Cr≤ 900 °C
Grade data

Aluminium

1060 · 3003
5052 · 6061

Sheet, coil, plate and tube for façades, signage, transport and heat exchange.

0.20–6.00 mmPlate to 150 mm
Alloy data