Automotive Exhaust
409L for the hot end, 439 for shells and mid-section, 436L where road salt and condensate collect. Coil and slit strip for tube mills and stampers.
Exhaust systems, appliance panels, kitchen equipment, façades, signage and heat exchangers. Six applications, six sets of demands — and the grade that answers each one.
The alloy is chosen per part, not per industry. Tell us what the part does — heat, salt, food contact, visible surface — and the quotation will name the material that survives it.
409L for the hot end, 439 for shells and mid-section, 436L where road salt and condensate collect. Coil and slit strip for tube mills and stampers.
304 and 430 for oven cavities, hoods and washer drums; 3003 fin stock for the heat exchanger behind them. 2B and BA finishes, film on both faces.
304 and 316L sheet in 2B or No.4, PVC-filmed for laser cutting and deep drawing without surface damage. Food-contact grades with full traceability.
No.4 and hairline stainless, PVDF-coated aluminium for cladding, soffits, column casings and handrails — coil or cut sheet, coated on both faces.
3003 and 5052 sheet in the flatness a wide-format printer needs — mill finish, PE-filmed, or coated on both faces for exterior boards.
Aluminium tube and fin stock for brazed exchangers, plus 436L and 444 stainless where condensate attacks the air side of the coil.
Photography shows the coil, strip and tube our customers process — not finished end products. Ask us for references in your specific application.
Slitting, cut-to-length, brushing and film lamination are arranged before the material is packed — so the strip that arrives is the strip your line can run.
A starting point for enquiry, not a design calculation. Final properties come from the mill test certificate issued for the heat you receive.
| Application | Recommended grade | Delivery form | Why this grade |
|---|---|---|---|
| Exhaust hot end | 409L · 441 | Coil, slit strip | Ti / Nb stabilised; scaling resistance to 800–950 °C at low alloy cost |
| Exhaust mid & rear | 439 · 436L | Coil, sheet | 18% Cr for oxidation; molybdenum where salt and condensate sit |
| Appliance panels | 304 · 430 | Coil, sheet | Formability and a finish that matches batch to batch |
| Kitchen & food equipment | 304 · 316L | Sheet, strip | Food-contact compliance, deep drawing, chloride cleaning |
| Façade & architecture | 304 · 316L · 5052 | Sheet, coil | Finish consistency; 5052 for coastal and marine air |
| Signage & panels | 3003 · 5052 · 1060 | Sheet, coil | Flatness, coating adhesion, weight |
| Heat exchange & HVAC | 3003 · 6063 · 436L | Tube, coil | Brazing behaviour and condensate resistance |
Grade recommendations assume continuous service in an oxidising atmosphere. Cyclic loading, welded joints and coastal exposure can change the answer — send the drawing.
Tell us the process, the environment and the volume. We will come back with a grade, a delivery form and the certificate that goes with it.