Molybdenum-bearing · 17.5% Cr ferritic

436L Stainless Steel

The corrosion specialist. One percent molybdenum lifts pitting resistance well above 409L and 439 — the difference that matters on salted roads, coastal cities and the Gulf climate.

0.75–1.25%Molybdenum
≈ 20PREN
≈ 850 °CMax service
2B · 2DFinish

436L

Chloride resistant

UNS S43600 · EN 1.4526 · JIS SUS 436L · ASTM A240

436L is a low-carbon, niobium- and titanium-stabilised ferritic stainless steel with 17.5% chromium and about 1% molybdenum. The molybdenum raises the pitting resistance equivalent number (PREN) to roughly 20, which is where it separates itself from the molybdenum-free grades.

In an exhaust system the enemy is rarely uniform rust — it is pitting under deposits of road salt, mud and acidic condensate. Muffler internals, flex connector bellows and the lower seam of a rear silencer are exactly where 436L earns its premium. For vehicles operating in the Gulf, along the Caspian, or on heavily salted winter roads, it is the specification that prevents warranty returns five years out.

Why specify 436L

  • PREN ≈ 20 versus ≈ 11–18 for 409L and 439 — a measurable jump in pitting resistance.
  • Retains useful strength and oxidation resistance to about 850 °C.
  • Dual stabilisation keeps weld zones free of sensitisation in thin bellows sections.
  • Performs in chloride-bearing condensate where 439 shows early pitting.
  • Slot-in alternative to 304 where nickel cost or thermal expansion is a problem.

Chemical composition

Typical ladle analysis, weight % — ASTM A240 / EN 10088-2
ElementCSiMnPSCrMoNiTiNbN
Range ≤ 0.025≤ 1.00≤ 1.00≤ 0.040≤ 0.030 16.00–18.000.75–1.25≤ 0.500.10–0.300.20–0.50≤ 0.025

Mechanical properties

Typical room-temperature properties, annealed and skin-passed
PropertyYield strength Rp0.2Tensile strength RmElongation A50Hardness
Value≥ 245 MPa≥ 410 MPa≥ 20%≤ 90 HRB

Supply range

FormThicknessWidth / sizeFinish
Cold-rolled coil0.30–2.50 mm600–1,250 mm2B, 2D
Cut sheet0.30–2.50 mm200–6,000 mm length2B
Slit strip0.30–2.00 mm8–1,200 mm2B, edge-conditioned
Welded tube0.40–1.50 mm wall25–100 mm ODAnnealed seam

Processing notes

Welding: match with a 436L or 444-type filler; keep interpass temperature low on bellows and thin tube. Forming: slightly higher springback than 409L — allowance in the die is normal. Pickling: if the weld is left unpolished, a light pickling pass restores full corrosion resistance on the seam. Cleaning: remove carbon-steel contamination before service; free iron is the usual cause of early rust on any ferritic grade.

Other grades

The rest of
the matrix.

409L

UNS S40910
EN 1.4512

Ti-stabilised 11% Cr for manifolds, downpipes and high-volume hot-end parts.

11% Cr≤ 800 °C
Grade data

439

UNS S43035
EN 1.4510

18% Cr dual-stabilised for muffler shells, converter housings and mid pipe.

18% Cr≤ 900 °C
Grade data

441

UNS S43940
EN 1.4509

Nb + Ti stabilised to 950 °C for close-coupled manifolds and flanges.

≤ 950 °CCreep
All grades