Titanium-stabilised · 11% Cr ferritic

409L Stainless Steel

The volume grade of the exhaust world. Low carbon plus titanium stabilisation keeps 409L ductile and weldable through repeated heat cycles — at the lowest alloy cost in the range we stock.

10.5–11.75%Chromium
0.07–0.30%Titanium
≈ 800 °CMax service
2B · 2DFinish

409L

Best value hot end

UNS S40910 · EN 1.4512 · JIS SUH 409L · ASTM A240

409L is a titanium-stabilised, 11% chromium ferritic stainless steel designed to resist high-temperature oxidation and thermal fatigue in automotive exhaust systems. The "L" denotes ultra-low carbon, which suppresses sensitisation in the weld heat-affected zone and keeps the as-welded structure tough.

In practice it is the material most exhaust programmes start with: manifolds, downpipes, front pipes and hot-end tubing. Where the thermal load or the chloride exposure rises, we step the specification up to 439, 441 or 436L — but for a large share of the system, 409L is the economically correct answer.

Why specify 409L

  • Titanium addition (min. 6 × carbon) prevents chromium carbide precipitation during welding.
  • Thermal expansion close to mild steel, so it welds to flanges and brackets without excessive distortion.
  • Oxidation resistance to roughly 800 °C in continuous exhaust service.
  • Excellent deep drawing and tube forming — routinely hydroformed and bent at room temperature.
  • Stable, predictable pricing compared with nickel-bearing austenitic grades.

Chemical composition

Typical ladle analysis, weight % — ASTM A240 / EN 10088-2
ElementCSiMnPSCrNiTiN
Range ≤ 0.030≤ 1.00≤ 1.00≤ 0.040≤ 0.030 10.50–11.75≤ 0.500.07–0.30≤ 0.030

Mechanical properties

Typical room-temperature properties, annealed and skin-passed
PropertyYield strength Rp0.2Tensile strength RmElongation A50Hardness
Value ≥ 205 MPa≥ 380 MPa≥ 22%≤ 90 HRB

Supply range

FormThicknessWidth / sizeFinish
Cold-rolled coil0.30–3.00 mm600–1,350 mm2B, 2D
Cut sheet0.30–3.00 mm200–6,000 mm length2B, 2D
Slit strip0.30–2.00 mm8–1,250 mm2B, edge-conditioned
Welded tube0.40–2.00 mm wall25–120 mm ODAs-welded, annealed seam

Processing notes

Welding: TIG, MIG and laser welding all suit 409L. Use a low-carbon ferritic filler (e.g. ER409 / ER409Cb) and keep heat input moderate; no preheat is required for thin gauge. Forming: bend radii of 1t–1.5t are typical for annealed strip. Heat treatment: anneal at 780–850 °C if a soft condition is needed; avoid slow cooling through 400–550 °C.

We can supply 409L with a certificate of origin, dimensional report and PMI verification per heat. If your programme requires a specific grain size or a tighter carbon ceiling, state it on the purchase order — we will source to it.

Other grades

Step up the heat
or the salt load.

439

UNS S43035
EN 1.4510

18% Cr, Ti + Nb stabilised. Mufflers, converter shells and mid-section pipe.

18% Cr≤ 900 °C
Grade data

436L

UNS S43600
EN 1.4526

17.5% Cr + 1% Mo for chloride pitting resistance in road-salt and coastal service.

1% MoSalt resistant
Grade data

441

UNS S43940
EN 1.4509

Nb + Ti stabilised, creep resistant to 950 °C for close-coupled manifolds.

≤ 950 °CCreep
All grades